Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 218 MPa
31600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP JCL36 PES (Europe-Africa-Middle East)
LNP* LUBRICOMP* JCL36 is a compound based on Polyethersulfone resin containing Carbon Fiber, PTFE. Added features include : Internally Lubricated, Electrically Conductive.
Flexural Yield Strength 218 MPa
31600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX153R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 218 MPa
31600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Yield Strength 218 MPa
31600 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..