Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 31.4 MPa | 4550 psi | ASTM D790 |
Samyang Trilen® 9550AC Polypropylene, General Purpose Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang. |