Mechanical Properties Metric English Comments
Flexural Yield Strength 212 MPa
30700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM SF2360 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
Flexural Yield Strength 212 MPa
30700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East)
LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic.