Flexural Yield Strength 299 MPa
43400 psi
ASTM D790
Samyang Tramid® 210G45 Polyamide, Reinforced
Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G45 is a reinforced grade.Applications:Automotive gear level housingConnectors..