Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 285 MPa | 41300 psi | ISO 178, ASTM D790 |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Flexural Yield Strength | 285 MPa | 41300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |