Polymer Property : Flexural Yield Strength = 279 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 110 - 279 MPa
16000 - 40500 psi
Average value: 207 MPa Grade Count:9
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..