Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 6.89 - 178 MPa | 1000 - 25900 psi | Average value: 132 MPa Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |