Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 16.2 MPa | 2350 psi | ASTM D790 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |
|||
Flexural Yield Strength | 16.2 MPa | 2350 psi | ASTM D790 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |