Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 219 MPa | 31800 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |