Mechanical Properties Metric English Comments
Flexural Yield Strength 217 MPa
31500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem ATX202R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 217 MPa
31500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Asia Pacific)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Yield Strength 217 MPa
31500 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Flexural Yield Strength 217 MPa
31500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Flexural Yield Strength 217 MPa
31500 psi
ASTM D790
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced
A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile ..
Copyright © lookpolymers.com All Rights Reserved