Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 211 MPa | 30600 psi | DIN 53455; ASTM D790 |
Kolon SPESIN® KP213G30 Flame Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Flexural Yield Strength | 211 MPa | 30600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific) LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie.. |
|||
Flexural Yield Strength | 211 MPa | 30600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon WEF42 PET/PBT LNP Stat-Kon WCF-1006 is a compound based on PET/PBT resin containing carbon and glass fiber reinforcements.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 211 MPa | 30600 psi | ASTM D790 |
Cheng Yu Plastic FV30G30 POM, 30% Glass Fiber |