Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 2.94 MPa | 427 psi | ASTM D638 |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |