Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 62.1 - 137 MPa | 9000 - 19800 psi | Average value: 111 MPa Grade Count:12 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |