Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 90.0 - 130 MPa @Temperature 80.0 - 80.0 °C |
13100 - 18900 psi @Temperature 176 - 176 °F |
Average value: 121 MPa Grade Count:9 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |