Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 92.0 - 1890 MPa | 13300 - 274000 psi | Average value: 921 MPa Grade Count:33 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |