Mechanical Properties Metric English Comments
Flexural Yield Strength 129 MPa
18700 psi
Bending Strength; ASTM D790
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Flexural Yield Strength 129 MPa
18700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® VIC4311 PBT
VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings.
Flexural Yield Strength 129 MPa
18700 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP J1000ER PES (Europe-Africa-Middle East)
LNP* THERMOCOMP* J1000ER is a compound based on Polyethersulfone resin. Added features include : Easy Molding, Mold Release
Flexural Yield Strength 129 MPa
18700 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Flexural Yield Strength 129 MPa
18700 psi
ASTM D790
PlastxWorld CEVIAN®-N GRSJ1 10% GF SAN resin
Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Yield Strength 129 MPa
18700 psi
ISO 178
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix
HexPly® 922-1 is a structural epoxy resin for general industrial applications and aerospace applications. HexPly® 922-1 has an exceptionally good hot/wet performance and a very high glass temperat..