Polymer Property : Flexural Yield Strength = 187 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 187 MPa
27100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX05050 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RX05050 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Yield Strength 187 MPa
27100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WFL28 PBT (Europe-Africa-Middle East)
LNP* LUBRICOMP* WFL28 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Flexural Yield Strength 187 MPa
27100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 187 MPa
27100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 187 MPa
27100 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Yield Strength 187 MPa
27100 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC
LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber.
Flexural Yield Strength 187 MPa
27100 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66
LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.