Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 169.6 MPa | 24600 psi | ASTM D790 |
Plenco 50240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black.. |