Mechanical Properties Metric English Comments
Flexural Yield Strength 83.0 - 166 MPa
12000 - 24100 psi
Average value: 109 MPa Grade Count:8
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..