Polymer Property : Flexural Yield Strength = 16510 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 49.6 - 113.8 MPa

@Temperature -40.0 - 71.0 °C
7190 - 16510 psi

@Temperature -40.0 - 160 °F
Average value: 81.7 MPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..