Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 103.1 MPa | 14950 psi | 15 mm/min; ASTM D790 |
LG Chemical 25SPR GPPS Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion.. |