Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 10.3 MPa @Strain 0.200 % |
1490 psi @Strain 0.200 % |
ASTM D790 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |
|||
Flexural Yield Strength | 10.3 MPa @Strain 0.200 % |
1490 psi @Strain 0.200 % |
ASTM D790 |
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C.. |