Polymer Property : Flexural Yield Strength = 14275 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 98.423 MPa
14275 psi
ASTM D790
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS
Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP..