Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 117.7 MPa | 17070 psi | ASTM D790; DIN 53455 |
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent
(discontinued **) Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009. |