Mechanical Properties Metric English Comments
Flexural Yield Strength 7.85 MPa
1140 psi
ASTM D790
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang.