Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 1.00 - 157 MPa | 145 - 22800 psi | Average value: 21.3 MPa Grade Count:14 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |