Polymer Property : Film Tensile Strength at Break, TD = 9360 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 64.5 MPa
9360 psi
ASTM D822
LyondellBasell Alathon® L5906 High Density Polyethylene
ApplicationsALATHON XL 5906 is a high molecular weight high density polyethylene homopolymer with a broad bimodal molecular weight distribution. This resin exhibits excellent stiffness, very high t..