Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 62.1 - 103 MPa | 9000 - 15000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OMBS (0.60 mil) Monoaxially Oriented, Co-Extruded Nylon6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 0.60 mil (15 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |
|||
Film Tensile Strength at Break, TD | 62.1 - 103 MPa | 9000 - 15000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ OMBS (1.00 mil) Monoaxially Oriented, Co-Extruded Nylon 6-Based Clear Film Description: Oxyshield™ Oriented Medium Barrier is a 1.00 mil (25 micron) monoaxially oriented, coextruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier throug.. |