Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 7.70 MPa | 1120 psi | Calculated from mfr's report of 20 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Film Tensile Strength at Break, TD | 7.70 MPa | 1120 psi | Calculated from mfr's report of 33 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |