Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 68.9 - 96.5 MPa | 10000 - 14000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ M-OPA (0.60 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Film Tensile Strength at Break, TD | 68.9 - 96.5 MPa | 10000 - 14000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ M-OPA (0.75 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Film Tensile Strength at Break, TD | 68.9 - 96.5 MPa | 10000 - 14000 psi | ASTM D882 |
Honeywell Capran® Oxyshield™ M-OPA (1.0 mil) Monoaxially Oriented, Co-Extruded In-Line Nylon6/Nylon6/Nylon6 Film Description: Capran® Oxyshield™ M-OPA (Machine Direction Oriented Polyamide) is a clear, monoaxially oriented, co-extruded in-line nylon6/nylon6/nylon6 film with high mechanical strength and.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 9990 psi | ASTM D882 |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882 |
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin Product Description: Exact 4160 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. These resins are designed for blown film applications requir.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882 |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882A |
DuPont Teijin Films Melinex® 3380 & CORE 1 Polyester Film Melinex® 3380 and Melinex® CORE1 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882A |
DuPont Teijin Films Melinex® CORE 1 & 3380 Polyester Film Melinex® CORE1 and Melinex® 3380 are one-side heat sealable, opaque white polyester films which are ideal in specialty laminated card applications. These films can be heat sealed to themselves and.. |
|||
Film Tensile Strength at Break, TD | 68.9 MPa | 10000 psi | ASTM D882 |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |