Polymer Property : Film Tensile Strength at Break, TD = 6770 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 46.7 MPa
6770 psi
ASTM D882
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin  (discontinued **)
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Film Tensile Strength at Break, TD 46.7 MPa
6770 psi
ASTM D882
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..
Film Tensile Strength at Break, TD 46.7 MPa
6770 psi
ASTM D882
ExxonMobil Exceed™ 3518 PA Premium Cast Film Resin
Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. ..