Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 46.2 MPa
6700 psi
ASTM D882
ExxonMobil EXACT™ 4053 Cast Plastomer
Product Description: Exact 4053 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed primarily for use in blends with poly..
Film Tensile Strength at Break, TD 46.2 MPa
6700 psi
ASTM D882
LyondellBasell Alathon® L4434 High Density Polyethylene
ApplicationsALATHON L 4434 is a medium molecular weight high density copolymer for use in blown film applications. Typical applications include blown film over pouches. Regulatory StatusL 4434 meet..