Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 45.4 MPa
6580 psi
ASTM D882
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed to provide blown film with low temperature sealability, good puncture resistance, optics and..