Film Tensile Strength at Break, TD 45.26 MPa
6565 psi
ASTM D882
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov..