Polymer Property : Film Tensile Strength at Break, TD = 6420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 44.3 MPa
6420 psi
ASTM D882
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene
For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Film Tensile Strength at Break, TD 44.3 MPa
6420 psi
ASTM D882
M. Holland Company MAGMA® LM311-D LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.