Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 44.2 MPa
6410 psi
Dow Elite® 5100 Linear Low Density Polyethylene
5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro..