Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 62.7 MPa
9100 psi
ASTM D882
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..