Film Tensile Strength at Break, TD 42.5 MPa
6170 psi
ASTM D882
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..