Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 38.2 MPa | 5540 psi | |
Kuraray HYBRAR® CF2 Mono Layer Cast Film Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Film Tensile Strength at Break, TD | 38.2 MPa | 5540 psi | ASTM D882 |
ExxonMobil LL 3001.32 Cast Film Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |