Film Tensile Strength at Break, TD 33.8 MPa
4900 psi
ASTM D882
Westlake LF2050 Hexene Linear Low Density Polyethylene
Westlake LF2050 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s..
Film Tensile Strength at Break, TD 33.8 MPa
4900 psi
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade
DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u..
Film Tensile Strength at Break, TD 33.8 MPa
4900 psi
Dow DOWLEX™ 2042A Linear Low Density Polyethylene, Food Grade
DOWLEX® 2042A Polyethylene resin offers good tear strength, medium stiffness and outstanding toughness for films used in food contact applications. When used unmodified and processed according to g..
Film Tensile Strength at Break, TD 33.8 MPa
4900 psi
ASTM D882
ExxonMobil Escorene® LD 721.IK Film Resin
Escorene Ultra LD 721 is a high vinyl acetate copolymer specialty film resin providing outstanding heat sealability, along with excellent strength properties and clarity.Availability: Latin America,..
Film Tensile Strength at Break, TD 33.8 MPa
4900 psi
ASTM D882
ExxonMobil Escorene™ FL 00218 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00218 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 240°C (464°F) may cause resin degradation. Machines should always b..