Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 49.2 MPa | 7130 psi | ASTM D882 |
Dow DOWLEX™ 2045.11G Linear Low Density Polyethylene For high speed, thin film applications Additional thermal stability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 49.2 MPa | 7140 psi | ASTM D882 |
ExxonMobil Exceed™ 3512CB Film Resin Exceed 3512CB resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3512CB resin have outstanding cold temperature toughness, impact strength and punc.. |