Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 46.1 MPa | 6690 psi | ASTM D882 |
NOVA Chemicals Sclair® 11L1 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion, food and liquid packaging.Data provided by the manufacturer.. |
|||
Film Tensile Strength at Break, TD | 46.1 MPa | 6690 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin
(discontinued **) Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng.. |
|||
Film Tensile Strength at Break, TD | 46.1 MPa | 6690 psi | |
Dow AFFINITY™ PL 1850 Polyolefin Plastomer AFFINITY® PL 1850 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistanc.. |