Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 45.1 MPa | 6540 psi | ASTM D882 |
Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Film Tensile Strength at Break, TD | 45.1 MPa | 6540 psi | ASTM D882 |
Chevron Phillips Dynex™ D508A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: superior dart impact, optical, hot-tack and heat seal properties, good drawdown, ca.. |
|||
Film Tensile Strength at Break, TD | 45.1 MPa | 6540 psi | ASTM D882 |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |