Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, TD = 4220 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 29.1 MPa
4220 psi
ASTM D882
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
Film Tensile Strength at Break, TD 29.1 MPa
4220 psi
ASTM D882
Braskem LQ 0518/21 AF LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Coextruded film for automatic packaging (FFS). Information provided by Braskem
Copyright © lookpolymers.com All Rights Reserved