Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 284 MPa | 41100 psi | ASTM D882 |
Formosa Plastics Formolene® L42009B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown file for either blending or extrusionBlown file for either blending or extrusionMeets all requirements of the U.S. Food and Drug Administration as spec.. |