Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 40.48 MPa | 5871 psi | ASTM D882 |
Dow DOWLEX™ 2083G Linear Low Density Polyethylene Excellent tear strength, outstanding toughness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |