Polymer Property : Film Tensile Strength at Break, TD = 396 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 2.73 MPa
396 psi
3M R3177 Repulpable Single-Coated Tapes
3M™ PTFE Glass Cloth Tape R3177 is a single-sided paper tapes coated with a patented, high tack transparent repulpable adhesive on one side and an easy release coating on the backside for smooth u..