Polymer Property : Film Tensile Strength at Break, TD = 3420 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 23.6 MPa
3420 psi
ASTM D882
ExxonMobil Pax-Plus™ 3208 Blown Film Resin
Pax-Plus 3208 is a rubber modified high density polyethylene film resin offering good physical properties with ease of processing. It exhibits toughness, stress crack resistance and low WVTR.Inform..