Polymer Property : Film Tensile Strength at Break, TD = 295 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 295 MPa
42800 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Bicor™ 70 SLP OPP Film
Product Description: Bicor 70 SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and lamina..