Polymer Property : Film Tensile Strength at Break, TD = 28800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 199 MPa
28800 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
ExxonMobil Metallyte™ 28MWHB OPP Film
Product Description: A multi-layer, cavitaed, white OPP film that has exceptional barrier to gases, flavors and moistures. It is metalized on one side with a proprietary sealant layer on the other. ..